    Technical Specification:
    Thickness: 20micron, 24micron
    Width: 150mm-1860mm
    Length: 150m-500m/1 "paper core; 1000m-4000m/3" paper core

    APPLICATION MANUAL
    1. Adjust rollor pressure and temperature according to different types of paper and ink.
    2. When using the film for the first time or changing to other thickness, we recommend a small trial volume before going into mass laminating.
    3. The following situation will affect the quality of laminating:
    A. Using metal ink.
    B. The ink contains too much wax, drying oil, anti-adhesive and silicon additive, etc.
    C. The ink is too thick.
    D. The ink is not completely dry.
    E. The humidity of paper is high.
    F. Too much powder.
    Process parameters 
    Equipment for lamination film;Dry and wet laminating machine
    Temperature:Normal:85℃-110℃
    Special:100℃-130℃
    Roller Pressure:10-18MPa
    Speed:8-50m/min
    Process parameters
    1.Adjust rollor pressure and temperature according to different types of paper and ink.
    2.When using the film for the first time or changing to other thickness,we recommend a small trial volume before going into mass laminating
    3.The following situation will affect the quality of laminating
    Using metal ink
    The ink contains too much wax,drying oil,anti-adhesive and silicon additive,etc
    The ink is too thick
    The ink is not completely dry
    The humidity of paper is high
    Too much powder