This is the plate characteristic for its high sensitivity, high resolution, wide developing tolerance and long run-length.
Photosensitive layer coated by imported photographic emulsion and resin.
Vacuum Ventilating Layer to greatly decreased exposure time.
Multi-Grain Layers, superior hydrophilicity, speedy ink-water balance and less water absorption.
Anodic oxidization give longer run-length.
Model
|
CXK-M8 positive PS plate
|
|
Exposure
|
Light source:
|
Yellow light
|
Exposure time:
|
60-80S(Based on:3000W.Iodine Gallium Lamp)
|
|
Fuji grey scale:
|
3rd step blank, 4th step inked ( The best exposure time)
|
|
Developing
|
Developer:
|
CXK-M28-DVP
|
Solution temperature:
|
25°C±1°C
|
|
Process time:
|
30-60S
|
|
CAUTION
|
1. Please renew or supplement the developer regularly pay attention to a proper solution density.
|
|
2. Please fix a reasonable exposure time according to actual light, power, brightness and other related.
|